SS304 (UNS S30400) is an austenitic stainless steel whose composition is defined per product standard, not by one universal set of numbers: ASTM A240 sheet and plate tables commonly specify carbon ≤0.07%, chromium 17.5–19.5% in many published editions while other A240 references list 18.0–20.0%, nickel 8.0–10.5%, manganese ≤2.00%, silicon ≤0.75% (some tables 1.00%), phosphorus ≤0.045%, sulfur ≤0.030% and nitrogen ≤0.10%, while ASTM A276 and A479 bar and forging tables often show carbon ≤0.08%, silicon ≤1.00% and chromium 18.0–20.0%, and EN 1.4301 is usually cited close to the A240 values with silicon commonly listed up to 1.00%. These are specification limits for a compliant heat, not the nominal "18/8" shorthand written on drawings; the edition and product form you invoke govern.
This page sets the limits side by side across standards, separates 304 from its low-carbon and high-carbon siblings, explains what each element does in the alloy, and shows how the Schaeffler equivalents and PREN turn chemistry into a screening decision. It closes with the two places where 304 chemistry is won or lost in practice: the mill test report and carbon control during MIM sintering. For the MIM-grade view, see MIM 304 stainless steel.
SS304 Composition Limits by Product Standard
The table below compares the limits commonly published for UNS S30400 in the three places buyers meet it: the ASTM A240 plate, sheet and strip table, the ASTM A276 (bars and shapes) and A479 (forged bar for pressure service) tables, and EN 1.4301. The differences look cosmetic on a drawing and are not cosmetic at incoming inspection — a heat at 0.078% carbon, 0.85% silicon and 18.6% chromium is compliant under the A276 bar table and not under A240.
| Element | ASTM A240 (S30400) | ASTM A276 / A479 | EN 1.4301 |
|---|---|---|---|
| Carbon (C) | ≤ 0.07 | ≤ 0.08 | ≤ 0.07 |
| Silicon (Si) | ≤ 0.75 (some tables 1.00) | ≤ 1.00 | ≤ 1.00 (verify edition) |
| Manganese (Mn) | ≤ 2.00 | ≤ 2.00 | ≤ 2.00 |
| Phosphorus (P) | ≤ 0.045 | ≤ 0.045 | ≤ 0.045 |
| Sulfur (S) | ≤ 0.030 (some editions 0.015–0.020) | ≤ 0.030 | ≤ 0.030 (verify edition) |
| Chromium (Cr) | 17.5–19.5 (some references 18.0–20.0) | 18.0–20.0 | 17.5–19.5 |
| Nickel (Ni) | 8.0–10.5 | 8.0–11.0 | 8.0–10.5 |
| Nitrogen (N) | ≤ 0.10 | often omitted; controlled separately | check edition |
| Iron (Fe) | balance | balance | balance |
Two cautions follow. The applicable edition and product form control: quote both on the purchase order, because a supplier working to A276 tables is not measuring against the A240 carbon cap, and published summaries of the same standard do not always agree. Nitrogen is inconsistently tabulated as well — many A240 304 tables list ≤0.10% while several A276 and A479 summaries omit it, even though it carries a 16× coefficient in the PREN formula below. Sulfur limits vary by edition as well (some 304 tables specify 0.015–0.020%), so quote standard and edition.
304 vs 304L vs 304H: The Carbon Number Splits the Family
All three grades are the same austenitic family; carbon is the lever that separates them, and it cuts both ways. Lower carbon suppresses chromium-carbide precipitation at grain boundaries when the steel sits in the roughly 450–850 °C sensitization window during welding or elevated-temperature service, protecting corrosion resistance in the affected zone. Higher carbon supports strength at temperature, which is why 304H exists.
| Grade | Carbon limit (wt %) | Primary intent | Watch-out |
|---|---|---|---|
| 304 (S30400) | ≤ 0.07 (A240) / ≤ 0.08 (A276, A479) | General corrosion-resistant austenitic grade | Higher carbon than L in welded, heavy-section service |
| 304L (S30403) | ≤ 0.030 | Welded and heavy-section construction; lower sensitization risk | Lower elevated-temperature strength than 304H; still not a chloride-service alloy |
| 304H (S30409) | 0.04–0.10 (commonly cited; verify edition) | Elevated-temperature strength | Minimum carbon is part of the requirement — verify in the purchase standard |
In practice, welded assemblies or heavy sections in corrosive service are normally specified as 304L, and the carbon cap is the reason; unwelded parts, or thin sections welded with controlled heat input, are usually served adequately by 304. 304H is a high-temperature engineering choice — its minimum carbon is mechanical rationale, not a corrosion decision, and the standard governs the range. A drawing revision that swaps grades needs chemistry, mechanical and delivery requirements re-checked together.
What Each Element Does in 304
Chromium, nominally 17.5–19.5% in A240 304, is the corrosion mechanism: it forms and repairs the passive chromium-oxide film. Chromium content alone does not set service life — surface finish, chloride exposure, temperature and fabrication history matter as much — and it is also a ferrite-forming term in weld-metal solidification calculations.
Nickel, nominally 8.0–10.5%, stabilizes the austenitic structure and contributes toughness and formability. It is the austenite-forming term in the Schaeffler nickel equivalent, and it is not the element responsible for pitting resistance — crediting nickel for chloride performance is a common specification error.
Carbon is the grade-defining element: ≤0.07% for A240 304, ≤0.030% for 304L, and 0.04–0.10% for 304H in commonly cited tables, with other editions using different minimum-carbon requirements — the purchase standard governs. In the Schaeffler nickel equivalent it is weighted 30×, a strong austenite former in solidification calculations, while in service it is the element that drives sensitization risk.
Manganese (≤2.00%) supports austenite stability and enters the nickel equivalent at half weight; it is a steelmaking and structure element, not a corrosion addition and not a substitute for nickel. Silicon (≤0.75% under A240, ≤1.00% under A276/A479 and EN 1.4301) is primarily a deoxidizer and a ferrite-forming term in the equivalents — which is why a silicon limit that differs across standards changes weld-metal predictions, not just paperwork.
Phosphorus (≤0.045%) and sulfur (≤0.030%) are controlled residuals. Sulfur is the trade-off element: in dedicated free-machining grades such as 303 it is deliberately raised to improve machinability, which makes those separate grades, not ordinary 304. In 304 itself sulfur is a residual that should not be pushed toward its limit, because sulfide inclusions can initiate pitting and degrade weldability. Nitrogen (commonly ≤0.10% where listed) strengthens the austenite and adds directly to pitting resistance.
Schaeffler Equivalents and PREN: Ranking Tools, Not Qualification
Two standard calculations reduce a chemistry table to a usable number. The Schaeffler equivalents — Cr_eq = Cr + Mo + 1.5Si + 0.5Nb and Ni_eq = Ni + 30C + 0.5Mn, in mass percent — predict weld-metal solidification mode and ferrite tendency. A representative 304 chemistry (Cr 18.5, Ni 8.5, C 0.05, Mn 1.5, Si 0.5, no Mo or Nb) lands at approximately Cr_eq 19.25 and Ni_eq 10.75, in the austenitic field — the practical reason 304 welds without ferrite-control problems.
- Schaeffler equivalents describe solidification and ferrite tendency, not corrosion performance in service.
- Coefficients differ between published versions of the diagram; state the formula whenever a number is reported.
- PREN for 304 is
Cr + 3.3Mo + 16N; with molybdenum near zero the index is driven almost entirely by chromium and nitrogen. - Nominal PREN from specification limits is a screening value, not the certified PREN of a heat.
| Calculation basis | Inputs | Result |
|---|---|---|
| Schaeffler equivalents, representative 304 | Cr 18.5, Ni 8.5, C 0.05, Mn 1.5, Si 0.5, Mo 0, Nb 0 | Cr_eq ≈ 19.25, Ni_eq ≈ 10.75 |
| PREN with typical nitrogen | Cr ≈ 18.5, Mo ≈ 0, N ≈ 0.05 | ≈ 19–20 |
| PREN from A240 Cr range, N = 0.10 | Cr 17.5–19.5, Mo 0 | ≈ 19.1–21.1 |
| Heat-specific | Certificate of analysis / powder-lot data | The only value defensible for qualification |
Read the numbers as ranking only. For 304-type chemistry the nominal index sits near 19–20, against roughly 23–29 for 316L depending on that alloy's actual chromium, molybdenum and nitrogen — the molybdenum gap, not a processing difference. That is also the grade's honest limitation: 304 is often unsuitable and normally not recommended for severe seawater, concentrated-chloride or crevice-prone service, though it can serve some milder chloride exposures depending on concentration, temperature and geometry — and no PREN from a nominal table changes that. For chloride service the material decision belongs one step up the alloy ladder; see MIM corrosion resistance and 316L stainless steel composition.
Verifying SS304 Chemistry on the Mill Test Report
Specification limits are only enforceable through the certificate. For stainless mill products that is normally an EN 10204 type 3.1 inspection certificate with the heat number and heat (cast) analysis; compare that analysis against the limits of the standard you actually invoked, element by element, where the margin is thin.
- Confirm the standard, edition and product form on the certificate match the purchase order — an A276 certificate does not satisfy an A240 carbon requirement.
- Check carbon first on L-grade or welded-service orders: the 0.030% cap is the point of specifying 304L.
- Check chromium and nickel against the invoked range; both are often reported to more digits than the drawing shows.
- Read nitrogen where the standard lists it — it moves PREN and is often missing from abbreviated certificates.
- Keep heat analysis and product analysis distinct: product analysis tolerances permit small deviations governed by the product standard.
MIM Context: Holding 304 Chemistry Through Sintering
In metal injection molding the certificate covers the powder, not the part. Between them sit the binder system, the debinding schedule and the sintering atmosphere, and carbon is the element most exposed to them: incomplete binder removal can leave residual carbon that enriches the part, while atmosphere chemistry decides whether the surface gains or loses carbon. Oxygen behaves similarly, affecting densification and surface chemistry.
The consequence for a 304 drawing is concrete: if the specification says 304 the carbon limit tolerates drift, but if it says 304L the 0.030% cap has to survive sintering — a process question, not a powder question. Powder-lot chemistry plus finished-part carbon and oxygen verification is the pair worth asking for. Emitech processes 304 alongside 316L, 17-4PH, 420 and 430L stainless, low-alloy steels and titanium on 17 MIM injection machines, 13 debonding furnaces and 22 sintering furnaces (4 continuous + 18 vacuum); sintered density runs 95–99% of theoretical, as-sintered tolerances ±0.3–0.5% of nominal dimension (about ±0.025 mm on features under 3 mm), with secondary operations to roughly ±0.01 mm. Chemistry for a specific part and lot is quoted on request — see MIM manufacturing capabilities, the MIM materials guide and 304 stainless steel in MIM.
Frequently Asked Questions
Q: What is the chemical composition of SS304 stainless steel?
Under ASTM A240 for sheet, plate and strip, UNS S30400 is commonly specified at carbon ≤0.07%, silicon ≤0.75%, manganese ≤2.00%, phosphorus ≤0.045%, sulfur ≤0.030%, chromium 17.5–19.5% in many published tables (other A240 references list 18.0–20.0%), nickel 8.0–10.5%, nitrogen ≤0.10%, iron balance, in weight percent. ASTM A276 and A479 bar tables commonly show carbon ≤0.08%, silicon ≤1.00% and chromium 18.0–20.0%, and EN 1.4301 is usually cited close to the A240 values with silicon commonly listed up to 1.00%. These are specification limits; a heat's certified chemistry comes from its certificate of analysis.
Q: Why does 304 show carbon ≤0.07% in ASTM A240 but ≤0.08% in A276 or A479?
Because the carbon cap belongs to the product standard, not to the grade name. A240 covers plate, sheet and strip, A276 covers bars and shapes, and A479 covers forged bar for pressure service; the same pattern applies to silicon (0.75% versus 1.00%) and chromium (17.5–19.5% versus 18.0–20.0%). Specify the standard, edition and product form on the purchase order, then inspect against that document.
Q: Should I specify 304L instead of 304 for welded parts?
Specify 304L when the assembly is welded and will see corrosive service, particularly in heavier sections or with high heat input that extends time in the sensitization range; the 0.030% carbon cap reduces chromium-carbide precipitation where intergranular corrosion starts. For unwelded parts, thin sections welded with controlled heat input, or elevated-temperature strength needs, 304 or 304H is usually the better fit. Carbon limit alone does not establish pressure-vessel or high-temperature suitability.
Q: Is 304 suitable for seawater or high-chloride service?
Usually not. With molybdenum near zero, the nominal pitting resistance index for 304 lands around 19–20, versus roughly 23–29 for 316L depending on its chemistry, and PREN ignores chloride concentration, temperature, crevice geometry and surface condition — the factors that dominate real pitting behavior. Severe seawater, concentrated-chloride or crevice-prone service is normally out of scope for 304 and belongs at 316L or a higher-molybdenum or duplex grade; some milder chloride exposures can work, but the call should rest on application-specific corrosion testing.
Q: How do I verify SS304 chemistry before accepting a shipment?
Ask for an EN 10204 type 3.1 inspection certificate with the heat number and heat analysis, then check it against the standard you actually invoked: carbon first for L-grade orders, then chromium, nickel and nitrogen, then residuals. Keep heat analysis and product analysis distinct: product analysis tolerances permit small deviations governed by the product standard. For MIM parts the powder certificate is only half the evidence — finished-part carbon and oxygen verification shows the chemistry survived sintering.
Composition tables are the starting point of a 304 specification and, on their own, a weak guarantee: the same nominal chemistry behaves differently depending on product standard, thermal history and, in MIM parts, carbon and oxygen control. If you are specifying SS304 or 304L parts and want the feedstock, sintering and verification detail, send the drawing through the contact page: Emitech reviews MIM suitability and returns a quotation within 24 hours.
Precision Metal Parts from Emitech
Nanjing Emitech delivers MIM, CNC machining, and custom metal parts. MIM services · Request a quote